MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Omnia Plastica PSU Polysulphone
Categories: Polymer; Thermoplastic; Polysulfone (PSU)

Material Notes: It is a non-reinforced amorphous polymer whose main features are its high thermal, electrical and mechanical properties which are typical of a crystalline polymer. Compared to its "brother" PES it has lower thermal properties, although this level is still high when compared to most other engineering plastics.

Features:

  • Resistance to high temperature.
  • Resistance to hydrolysis and steam.
  • Mechanical properties : tensile stress, flexural strength, E.modulus
  • Chemical resistance
  • Electrical properties
  • Transparency
Weak Point:

The cost is higher than conventional engineering plastics. It does not stand UV rays and is therefore not suitable for outdoor applications.

Application:

  • Electrical: the very good insulating and dielectric properties make it irreplaceable in many electrical applications: plates for circuits, coils, insulators.
  • Mechanical: it is used for high performance applications such as bearings and precision gears at low as well as high temperatures.
  • Chemical: the use in this field is ideal thanks to its high chemical and thermal resistance. Good resistance to mineral acids, alkali and salt solutions. PSU is attacked by esters, chlorine and aromatic hydrocarbons.
  • Food contact: it is physiologically inert and is therefore used for parts in contact with food, even at high temperature. The excellent chemical properties make it suitable for pump components, flanges, etc. which are in contact with food liquids.

Information provided by Omnia Plastica s.p.a. for semifinished products such as sheet, rod, and tube.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 g/cc0.0448 lb/in³ISO.1183 DIN.53479
Moisture Absorption at Equilibrium 0.30 %0.30 %50% relative humidity
Water Absorption at Saturation 0.60 %0.60 %23°C
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 6969dry sample; ISO2039.2
Ball Indentation Hardness 140 MPa20300 psiISO2039.1 DIN.53456
Tensile Strength at Break 70.0 MPa10200 psiISO.527 DIN.53455
Elongation at Break >= 50 %>= 50 %ISO.527 DIN.53455
Tensile Modulus 2.50 GPa363 ksiISO.527 DIN.53455
Compressive Strength 13.0 MPa1890 psi1% strain over 1000 hours; ISO.899 DIN.53444
Charpy Impact Unnotched NBNB7.5 J; ISO.R179 DIN.53453
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²ISO179/3C DIN.53453
Coefficient of Friction, Dynamic 0.450.45on dry ground steel; load =0.05MPa; speed =0.6 m/s
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.10e+11 ohm-cm2.10e+11 ohm-cmISO.93 DIN.53482
Dielectric Constant 3.1
@Frequency 1e+6 Hz
3.1
@Frequency 1e+6 Hz
ISO.250 DIN.53483
Dielectric Strength 25.0 kV/mm635 kV/inISO.243 DIN.53481
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
ISO.250 DIN.53483
 
Thermal PropertiesMetricEnglishComments
CTE, linear 60.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
33.3 µin/in-°F
@Temperature 73.4 - 140 °F
Thermal Conductivity 0.260 W/m-K1.80 BTU-in/hr-ft²-°FDIN.52612
Maximum Service Temperature, Air 150 °C302 °FContinuous; 5000 hours based on a tensile stress of 50% at 23° C.
 180 °C356 °Fshort period, no load
Deflection Temperature at 1.8 MPa (264 psi) 174 °C345 °FISO.75 DIN.53461
Minimum Service Temperature, Air -50.0 °C-58.0 °Fimpact conditions and heavy loads not considered
Flammability, UL94  HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 V-2
@Thickness 6.00 mm
V-2
@Thickness 0.236 in
Oxygen Index 32 %32 %ISO.4589
 
Descriptive Properties
FormAmorphous

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA)
Overview of materials for Polyether Block Amide (PEBA)
Overview of materials for Polyetherimide (PEI), 10% Glass Fiber
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled

POMNIA29 / 55620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.