MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
2-Methylbutane, C5H12
Categories: Fluid; Solvent

Key Words: C5H12
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.620 g/cc
@Temperature 20.0 °C
Viscosity 0.217 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 72.151 g/mol
Vapor Pressure 574.895 torr
@Temperature 20.0 °C
Surface Tension 13.7 dynes/cm
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 33.4 atm
Critical Temperature 187 °C
Critical Density 0.236 g/cc
Critical Molar Volume 306 cm³/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 342.1 J/g
Specific Heat Capacity 1.645 J/g-°C
@Temperature 25.0 °C
Vapor
Melting Point -159.9 °C
Boiling Point 27.9 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.351
@Wavelength 589.3 nm
nD
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter15.6338
Antoine's Vapor Pressure B Parameter2348.67
Antoine's Vapor Pressure C Parameter-40.05
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)78-78-4
Chemical FormulaC5H12
Critical Compressibility (Zc)0.271
Dipole moment (p/C.m)3.336E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A367.32
Dynamic Viscosity Parameter B191.58
Molar Heat Capacity (298K)118.694 J/mol-K
Molar Heat Capacity of Vapor a Parameter-9.5186
Molar Heat Capacity of Vapor b Parameter0.5063
Molar Heat Capacity of Vapor c Parameter-0.0002728
Molar Heat Capacity of Vapor d Parameter5.72E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1265

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LG Chemical Propylene
Hexane (C6H14)
Ethane, C2H6
Butane (C4H10)
Acetylene, Ethyne, C2H2

VORGS259 / 99622

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.