MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ethane, C2H6
Categories: Fluid

Key Words: C2H6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.5446 g/cc
@Temperature -89.0 °C
0.01967 lb/in³
@Temperature -128 °F
Liquid
Molecular Weight 30.07 g/mol30.07 g/mol
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0110 W/m-K
@Temperature -73.1 °C
0.0763 BTU-in/hr-ft²-°F
@Temperature -99.7 °F
gas at saturation vapor pressure
 0.0213 W/m-K
@Pressure 0.100 MPa,
Temperature 26.9 °C
0.148 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 80.3 °F
gas
 0.0354 W/m-K
@Pressure 0.100 MPa,
Temperature 127 °C
0.246 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 260 °F
gas
 0.0522 W/m-K
@Pressure 0.100 MPa,
Temperature 227 °C
0.362 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 440 °F
gas
 0.0705 W/m-K
@Pressure 0.100 MPa,
Temperature 327 °C
0.489 BTU-in/hr-ft²-°F
@Pressure 14.5 psi,
Temperature 620 °F
gas
Melting Point -182.8 °C-297.0 °F
Boiling Point -88.6 °C-127 °F
 
Descriptive Properties
CAS Number74-84-0

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Methane (CH4)
Propane (CH3CH2CH3)
Oxygen (O2)
Nickel Aluminide, NiAl
n-Heptane, C7H16

VORG017m / 178229

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.