MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Johnson Matthey Matti-phos 15 Alloy for Fluxless Brazing of Copper  (discontinued **)
Categories: Metal; Nonferrous Metal; Copper Alloy; Solder/Braze Alloy

Material Notes: This alloy gives ductile joints on copper to copper and is used by electrical assemblies such as motors and contacts.

Optimum Joint Gap 0.05 - 0.2 mm.
AWS A5.8-92 BCuP-5
BS EN 1044 1999 CP102; Does not conform exactly to the requirements of EN 1044.
Federal Specification QQ-B-650 BCuP-5
Equivalent to Engelhard Silvaloy 15
Equivalent to Handy & Harman Sil-Fos 15
Equivalent to J W Harris Stay-Silv 15

Information provided by Johnson Matthey.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesOriginal ValueComments
Melting Point 645 - 800 °C
Solidus 645 °C
Liquidus 800 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 80 %
Phosphorus, P 5.0 %
Silver, Ag 15 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ChevronTexaco SAE 75W-90 Manual Transaxle Fluid GL-4
AISI 1045 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/320 Polyolefin
Universal Wire Works Au-Pd-Ni (AMS 4784) Gold Brazing Filler Metal
Universal Wire Works BAu-5 (AMS 4785) Gold Brazing Filler Metal

NJMMJ19 / 17625

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.