MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco SAE 75W-90 Manual Transaxle Fluid GL-4
Categories: Fluid; Lubricant

Material Notes: Features

Chevron Manual Transaxle Fluid GL-4 is a multipurpose lubricant.

Chevron Manual Transaxle Fluid GL-4 is formulated with ISOSYN® base stocks and synthetic polymer to meet the severe demands of both cold and hot weather operations. It contains a carefully balanced sulfurphosphorus extreme pressure additive package to provide maximum gear protection, long lubricant life, and superior thermal and oxidation stability. In addition, this lubricant is fortified with rust and corrosion inhibitors, a foam inhibitor, and a pour point depressant.

Applications

Chevron Manual Transaxle Fluid GL-4 is recommended for use in all manual transmissions and manual shift transaxles requiring SAE 75W-90, API GL-4 lubricants. Its multiviscosity characteristics allow smooth shifting over a broad ambient temperature range.

Chevron Manual Transaxle Fluid GL-4 meets the performance requirements of API Service Category GL-4.

Key Words: CPS Number: 250260; MSDS Number: 8567
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 29 °29 °
Brookfield Viscosity 40000 cP
@Temperature -40.0 °C
40000 cP
@Temperature -40.0 °F
Viscosity Measurement 195195Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 650 SUS650 SUS
Saybolt Viscosity at 210°F 107 SUS107 SUS
Kinematic Viscosity at 40°C (104°F) 128.3 cSt128.3 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 21.5 cSt21.5 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -42.0 °C-43.6 °FASTM D97

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1045 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
ChevronTexaco RPM® SAE 140 Gear Oil
Johnson Matthey Matti-phos 15 Alloy for Fluxless Brazing of Copper
Syensqo (Solvay Specialty Polymers) Cogegum® GFR/320 Polyolefin
Envalior Arnitel® CM600-V TPC-ES FR

WCHEV207 / 74822

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.