MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Finathene® 53080 HDPE, blow molding, sheet  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Finathene E® 53080 is a high density polyethylene produced by the slurry loop low pressure polymerization process.

Finathene E® 53080 has been especially developed for the production of containers to be submitted to the regulations for transportation of dangerous goods.

Finathene® 53080 is best processed at temperatures between 180 and 220°C.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccISO 1183
Environmental Stress Crack Resistance 200 hourASTM D1693-70
High Load Melt Index 8.0 g/10 min
@Load 21.6 kg
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38.0 MPaISO 527
Tensile Strength, Yield 28.0 MPaISO 527
Elongation at Break >= 700 %ISO 527
Elongation at Yield 9.0 %ISO 527
Flexural Modulus 1.30 GPaISO 178
Tensile Impact Strength 120 kJ/m²Notched, -30°C; ISO 8256
 280 kJ/m²Notched, 23°C; ISO 8256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 127 °CISO 306
 
Descriptive Properties
Food ApprovalThis material complies with the main regulations concerning non-toxicity of plastics materials in contact with food stuffs.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5840 High Density Polyethylene
Total 54050 HDPE, blow molding
Chevron Phillips Marlex® 9515H High Density Polyethylene, Blow Molding
Chevron Phillips Marlex® 9509HF High Density Polyethylene, Blow Molding
FKuR Kunststoff Bio-Flex® F 6514 PLA Blend

PFINAP059 / 38642

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.