MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total 54050 HDPE, blow molding
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: Applications: 55-gallon shipping containers, open-top drums, industrial tanks, agricultural chemical tanks.

Blow Molding Stock Temperature 380 – 450 ºF

Extrusion melt temperature 400 - 480ºF

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.954 g/cc0.0345 lb/in³ASTM D 792
Environmental Stress Crack Resistance >= 200 hour>= 200 hourASTM D1693 cond. B 10% lgepal
 >= 1000 hour>= 1000 hourASTM D1693 cond. B 100% lgepal
High Load Melt Index 5.5 g/10 min
@Load 21.6 kg
5.5 g/10 min
@Load 47.6 lb
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 39.3 MPa>= 5700 psiASTM D 638 type IV
Tensile Strength, Yield >= 28.3 MPa>= 4100 psiASTM D 638 type IV
Elongation at Break >= 600 %>= 600 %ASTM D 638, type IV
Flexural Modulus 1.31 GPa190 ksiASTM D 790
Izod Impact, Notched 6.67 J/cm
@Thickness 3.17 mm
12.5 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 128 °C263 °FASTM D3417

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Alathon® L5840 High Density Polyethylene
Baystar™ 50100.1 HDPE blow molding
Total 49080 UV HDPE blow molding
Total MS 201 B N HDPE blow molding
Braskem HB 0155 HDPE Blow Molding Polyethylene

PFINAP061 / 38644

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.