MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Network Polymers PC-1035
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Description: Injection Molding Grade Low Gloss Polycarbonate

Information provided by Network Polymers Inc.

A. Schulman has acquired Network Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.18 g/cc1.18 g/ccASTM D792
Melt Flow 23 g/10 min
@Load 3.80 kg,
Temperature 230 °C
23 g/10 min
@Load 8.38 lb,
Temperature 446 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 71.7 MPa10400 psichs 2 in/min; ASTM D638
Flexural Strength 105.8 MPa15350 psiStress at 5% Strain, Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Flexural Modulus 2.76 GPa401 ksiTest Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched NBNBTest Method A (0.125 in bar); ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 108 °C226 °F0.125 in bar; ASTM D648
Vicat Softening Point 135 °C275 °F0.125 inch bar, 1 Kg; ASTM D1525
Flammability, UL94  V-2
@Thickness 1.57 mm
V-2
@Thickness 0.0620 in
All Colors
 V-2
@Thickness 3.17 mm
V-2
@Thickness 0.125 in
All Colors

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polycarbonate, Molded
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Solvay PEEK Laminates
Overview of materials for Polyetheretherketone, Glass Fiber Filled
Overview of materials for Polyetheretherketone, Carbon Fiber Filled

PDIAM142 / 29980

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.