MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trimay® Wear Plate T157 Iron-based Steel Overlay
Categories: Ceramic; Carbide; Metal; Ferrous Metal; Alloy Steel

Material Notes: Overlay Description: T157 is a iron-based steel overlay wear solution with a unique proprietary chemical composition designed to withstand heavy wear environments exposed to mild-moderate direct impact. T157 is the top-performing chromium carbide wear plate on the market. It has a smooth surface, like T138 and T156 overlays, plus extra Chromium and Manganese gives T157 up to 30% more wear resistance than the T156.

Overlay Attributes: T157 consistently rates between 56 - 58 HRc for hardness, and only loses 0.13 g (+/-0.03) on ASTM G65-04 Procedure A mass loss test. T157 has a slick drag coefficient of 0.185 to deter material buildup, and it lasts up to 30% longer than Trimay’s T156.

Common Application: T157 is the best wearing chromium carbide overlay offered and it performs best in heavy wear environments exposed to mild or moderate direct impact. T157 wears longer than Trimay’s other chrome overlays (T138 & T156), and, in some cases, it is more practical than using complex or tungsten wear plates (like Trimay’s T161 or T170) which sometimes overperform and outlive their purpose. T157 is often used for coal handling and conveyor applications.

Information provided by Trimay®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 8000 micronsStandard (single pass)
 <= 17000 microns
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 56 - 58
K Factor (Wear Factor) 0.10 - 0.16[g], 6000 cycles mass loss; ASTM G65-04 Procedure A
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 4.0 %
Chromium, Cr <= 30 %
Iron, Fe >= 62 %
Manganese, Mn <= 2.0 %
Molybdenum, Mo <= 2.0 %
 
Descriptive Properties
Substrate Materials44W(or 300W) steel
 516 Grade 70 for pressure
 Stainless Steel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trimay® Wear Plate T161 Iron-based Steel Overlay
Trimay® Wear Plate T156 Iron-based Steel Overlay
Trimay® Wear Plate T171 Iron-based Steel Overlay
Trimay® Wear Plate T170 Nickel-based Steel Overlay
Zirconium Carbide, ZrC

NTRIM002 / 120816

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.