MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trimay® Wear Plate T161 Iron-based Steel Overlay
Categories: Ceramic; Carbide; Metal; Ferrous Metal; Alloy Steel

Material Notes: Overlay Description: T161 is a iron-based steel overlay wear solution with a unique alloy composition designed to resist heavy wear under extreme temperature. This is Trimay’s complex carbide overlay that deters corrosion and protects against abrasion even in extreme heat.

Overlay Attributes: T161 consistently rates between 60-62 HRc for hardness, and only loses 0.11 g (+/-0.03) on ASTM G65-04 Procedure A mass loss test. The mixture of Chromium Iron, Niobium and Vanadium, plus Trimay’s Sub Arc Welding process, forms a tight crystalline structure, giving T161 the ability to resist corrosion and heavy wear between temperatures of 450o C & 650o C. Common Application:

T161 is primarily used for hot or corrosive wear environments. The Oil and Gas, Concrete and Power Industries are primarily where T161 is used. A variation of the T161, the T161i, has added nickel and is used for moderate-heavy impact environments.

Information provided by Trimay®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 8000 microns315 milStandard (single pass)
 <= 14000 microns<= 551 mil
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 56 - 5856 - 58
K Factor (Wear Factor) 0.080 - 0.140.080 - 0.14[g], 6000 cycles mass loss; ASTM G65-04 Procedure A
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 4.0 %<= 4.0 %
Chromium, Cr <= 22 %<= 22 %
Iron, Fe >= 57.5 %>= 57.5 %
Manganese, Mn <= 1.5 %<= 1.5 %
Molybdenum, Mo <= 6.0 %<= 6.0 %
Niobium, Nb (Columbium, Cb) <= 6.0 %<= 6.0 %
Tungsten, W <= 2.0 %<= 2.0 %
Vanadium, V <= 1.0 %<= 1.0 %
 
Descriptive Properties
Substrate Materials44W(or 300W) steel
 516 Grade 70 for pressure
 Stainless Steel

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trimay® Wear Plate T157 Iron-based Steel Overlay
Trimay® Wear Plate T156 Iron-based Steel Overlay
Trimay® Wear Plate T170 Nickel-based Steel Overlay
Trimay® Wear Plate T171 Iron-based Steel Overlay
NeoGraf eGRAF® SPREADERSHIELD™ SS400 Graphite

NTRIM003 / 120817

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.