MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Celanese Vectra® C550 Liquid Crystal Polymer (LCP), 50% Mineral Filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes:

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.89 g/ccISO 1183
Water Absorption 0.020 %Immersion to equilibrium; ISO 62
Moisture Absorption at Equilibrium 0.020 %ISO 62
Linear Mold Shrinkage 0.0030 cm/cm
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 115 MPaISO 527
Elongation at Break 2.4 %IEC 527
Tensile Modulus 19.0 GPaISO 527
Flexural Strength 170 MPaISO 178
Flexural Modulus 17.0 GPaISO 178
Compressive Strength 95.0 MPa1% Deflection, ISO 604
Compressive Modulus 16.5 GPaISO 604
Izod Impact, Notched (ISO) 0.500 J/cm²ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²ISO 179
Tensile Impact Strength 50.0 kJ/m²Notched; ASTM D1822
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 ohm-cmIEC 93
Surface Resistance 1.00e+16 ohmIEC 93
Dielectric Constant 3.7
@Frequency 1e+7 Hz
 4.0
@Frequency 1000 Hz
IEC 250
Dissipation Factor 0.0070
@Frequency 1e+7 Hz
 0.020
@Frequency 1000 Hz
IEC 250
Arc Resistance 183 sec
Comparative Tracking Index 225 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 1.00 µm/m-°C
@Temperature -50.0 - 200 °C
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -50.0 - 200 °C
Melting Point 325 °CISO 3146
Maximum Service Temperature, Air 130 °CGeneric Rating for Vectra LCP
Deflection Temperature at 1.8 MPa (264 psi) 225 °CISO 75/A
UL RTI, Electrical 130 °CGeneric Rating for Vectra LCP
UL RTI, Mechanical with Impact 130 °CGeneric Rating for Vectra LCP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese ZENITE 5145L LCP, 45% Glass Reinforced
Celanese ZENITE 6635 LCP, 40% Mineral / Glass Reinforced (Extended Stress-Strain Tabular Data)
Dow Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Celanese VECTRA® 2355MT Carbon Fiber Reinforced Liquid Crystal Polymer (LCP)
Celanese VECTRA S135 LCP, 35% Glass Reinforced

PHCV03 / 45843

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.