MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Elvax® resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range without the need for plasticizers.

Elvax® resins can be used alone or to improve the flexibility, resilience and toughness of other resins. Depending on the demands of the particular application, they can be pigmented, foamed, filled, and/or crosslinked. In addition to their performance advantages, Elvax® resins are processed easily using conventional thermoplastic processing techniques, i.e., injection molding, extrusion and foaming, as well as rubber processing techniques, i.e., Banbury mixing, foam extrusion and molding.

Test specimens except for tensile impact where prepared by compression molding (ASTM D1928, procedure C). Tensile impact samples were injection molded.

Processing Information:

Molding and Extruding

Modified and unmodified Elvax® resins can be processed in conventional thermoplastic and rubber processing equipment. The temperature profile will vary with machine type, size and screw design as well as with part size, thickness or configuration.

Compounding

Elvax® resins are compatible with a variety of other resins and elastomers including polyethylene, polypropylene and styrene-butadiene rubber. Clays and other inorganic fillers can be added to improve abrasion resistance and lower cost.

Foaming Agents

Elvax® resins are readily foamed using chemical or physical blowing agents.

Crosslinking Agents

Peroxides such as "Di-Cup"† and "Vul-Cup"† dicumyl peroxide can be used to crosslink or vulcanize Elvax® resins.

(†Hercules Inc.)

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.951 g/cc0.0344 lb/in³ASTM D792
Vinyl Acetate Content 28 %28 %TGA
Melt Index of Compound 25 g/10 min25 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D2240
Hardness, Shore D 2828ASTM D2240
Tensile Strength, Ultimate 9.00 MPa1310 psiType IV, crosshead speed 2 in/min; ASTM D638
 1.40 MPa
@Temperature 49.0 °C
203 psi
@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
 23.0 MPa
@Temperature -20.0 °C
3340 psi
@Temperature -4.00 °F
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
Elongation at Break 850 %850 %Type IV, crosshead speed 2 in/min; ASTM D638
 400 %
@Temperature -20.0 °C
400 %
@Temperature -4.00 °F
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638
 500 %
@Temperature 49.0 °C
500 %
@Temperature 120 °F
Type IV, crosshead speed 2 in/min; ASTM D638
Modulus of Elasticity 0.0110 GPa1.60 ksi
 0.0460 GPa
@Temperature -20.0 °C
6.67 ksi
@Temperature -4.00 °F
Flexural Modulus 0.0110 GPa1.60 ksiASTM D790
 0.00620 GPa
@Temperature 49.0 °C
0.899 ksi
@Temperature 120 °F
ASTM D790
 0.0790 GPa
@Temperature -20.0 °C
11.5 ksi
@Temperature -4.00 °F
ASTM D790
Flexural Stiffness 11.00 MPa1595 psi
 46.00 MPa6672 psi
Tensile Impact Strength  485 kJ/m²
@Temperature -20.0 °C
231 ft-lb/in²
@Temperature -4.00 °F
ASTM D1822
 670 kJ/m²
@Temperature 23.0 °C
319 ft-lb/in²
@Temperature 73.4 °F
ASTM D1822
Compression Set 100 %
@Temperature 70.0 °C
100 %
@Temperature 158 °F
Method B, 22 hours; ASTM D395
 60 %
@Temperature 25.0 °C,
Time 864000 sec
60 %
@Temperature 77.0 °F,
Time 240 hour
Method B; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 42.0 °C108 °FASTM D1525
Brittleness Temperature <= -100 °C<= -148 °FASTM D762
 
Processing PropertiesMetricEnglishComments
Processing Temperature 121 - 204 °C250 - 399 °F
 
Descriptive Properties
Cycle time0.5-2 minutesMolding, equipment and part design dependent
Vinyl Acetate Content28 wt.%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin
Celanese Ateva® 2820A Ethylene Vinyl Acetate Copolymer
Dow Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin
Dow Elvax® 350 Ethylene Vinyl Acetate
Celanese Vectra® C550 Liquid Crystal Polymer (LCP), 50% Mineral Filled

PDUPM121 / 33788

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.