Product Description: ExxonMobil™ LD 2023 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or cast film equipment. LD 2023 resins can be drawn down to 1.0 mil gauge Availability: Asia Pacific; Latin America; North America Additive: Antiblock: 1000 ppm; Slip: 750 ppm; Thermal Stabilizer: Yes Applications: Blend Partner; Bread Bags; Display Packaging Film; Food Packaging; Form Fill And Seal Packaging; Freezer Film; High Clarity Film; High Quality Lamination; Lamination Film; Laundry Film; Light Duty Shrink Film; Produce Bags; Salad Bags; Textile Packaging Information provided by ExxonMobil |