Product Description: LD 157CW offer good mechanical properties as well as excellent opticals. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications: - Co-Extrusion Films
- Label Film
- Lamination Film
- Medium Duty Shrink Film
- Overwrap Film
Information provided by ExxonMobil |