MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Hanwha Azdel Plus R401B02N 40% Continuous Random Fiber Mat / PP Resin Matrix
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: AZDEL® R401B02N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a basic homogeneous fiber distribution. This material is typically used for standard semi-structural applications.

Commercially available only to European based customers.

Information provided by Azdel.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccLaminate; ISO 2577
 1.24 g/ccMolded plaque; ISO 2577
Filler Content 40 %AZDEL Test
Thickness 3900 micronsAZDEL Test
Linear Mold Shrinkage 0.0027 cm/cm320 x 320 mm flat plaque; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 90.0 MPaISO 527/4
Elongation at Break 2.2 %ISO 527/4
Tensile Modulus 5.60 GPaISO 527/4
Flexural Strength 150 MPaISO 178
Flexural Modulus 5.70 GPaISO 178
Charpy Impact, Notched 8.50 J/cm²ISO 179/2fn
Impact 5500
@Thickness 4.00 mm
N; Multi-axial at max. force; ISO 6603-2
Impact Test 15.0 J
@Thickness 4.00 mm
Multi-axial, at max. force; ISO 6603-2
 45.0 J
@Thickness 4.00 mm
Multi-axial, total energy; ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.0 µm/m-°C
@Temperature 0.000 - 120 °C
100 x 15 x 3 mm sample; AZDEL Test
 43.0 µm/m-°C
@Temperature -30.0 - 0.000 °C
100 x 15 x 3 mm sample; AZDEL Test
Melting Point 114 °CRecrystallizing temperature; ISO 3146
 166 °CISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 158 °CISO 75/2a
 
Processing PropertiesOriginal ValueComments
Processing Temperature 205 - 220 °CSurface temperature
Mold Temperature 30.0 - 90.0 °C
Back Pressure 15.0 - 25.0 MPaDepending on wall thickness and part complexity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient OnForce™ LFT PP-40 LGF/000 Natural PP Homopolymer with 40% Long Glass Fiber
Hanwha Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix

PZZGEAZ79 / 40628

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.