MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient OnForce™ LFT PP-40 LGF/000 Natural PP Homopolymer with 40% Long Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Glass Fiber Filler

Material Notes: PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. These products exhibit enhanced physical and mechanical properties versus standard short fiber products. Benefits of LFT compounds include improved impact strength, elastic modulus, and material strength across wide temperature ranges from subambient to highly elevated. Furthermore, LFT compounds have been shown to offer improved performance in the areas of creep and fatigue performance, improved dimensional stability, and exhibit an exceptional surface finish when compared to traditional highly filled short fiber products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Filler Content 40 %40 %Long Glass Fiber
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 118 MPa17100 psiType I, 5.1 mm/min; ASTM D638
Elongation at Break 2.5 %2.5 %Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 8.76 GPa1270 ksiType I, 5.1 mm/min; ASTM D638
Flexural Strength 190 MPa27600 psiASTM D790
Flexural Modulus 7.58 GPa1100 ksiASTM D790
Izod Impact, Notched 1.76 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
3.30 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256
Dart Drop, Total Energy  5.76 J
@Thickness 3.18 mm,
Temperature -20.0 °C
4.25 ft-lb
@Thickness 0.125 in,
Temperature -4.00 °F
2.20 m/sec; Injection Molded, Energy to Max Load; ASTM D3763
 6.34 J
@Thickness 3.18 mm,
Temperature 23.0 °C
4.68 ft-lb
@Thickness 0.125 in,
Temperature 73.4 °F
2.20 m/sec; Injection Molded, Energy to Max Load; ASTM D3763
 13.7 J
@Thickness 3.18 mm,
Temperature -20.0 °C
10.1 ft-lb
@Thickness 0.125 in,
Temperature -4.00 °F
2.20 m/sec; Injection Molded; ASTM D3763
 14.0 J
@Thickness 3.18 mm,
Temperature 23.0 °C
10.3 ft-lb
@Thickness 0.125 in,
Temperature 73.4 °F
2.20 m/sec; Injection Molded; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C
@Thickness 3.18 mm,
Temperature -30.0 - 30.0 °C
11.1 µin/in-°F
@Thickness 0.125 in,
Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
@Thickness 3.18 mm
315 °F
@Thickness 0.125 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 221 °C410 - 430 °F
Mold Temperature 65.6 °C150 °F
Drying Temperature 93.3 °C
@Time 7200 sec
200 °F
@Time 2.00 hour
 
Descriptive Properties
FormsPellets
Generic NamePolypropylene Homopolymer
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PlastiComp Complet® LGF40 - PP Homopolymer Polypropylene, 40% Long Glass Fiber Reinforced
PlastiComp Complet® LGF30 - PP Homopolymer Polypropylene, 30% Long Glass Fiber Reinforced
Envalior Durethan® BKV 230 H2.0 DUS008 000000 Nylon 6 (PA6), 30% Glass Fiber Reinforced, Conditioned
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Overview of materials for Polypropylene with 40% Glass Fiber Filler

PH1PN9426 / 103262

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.