A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applications. This grade of Geolast TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding, extrusion or blow molding. It is polyolefin based and completely recyclable. Recyclable. Designed for improved fluid resistance. Information provided by ExxonMobil and predecessor Advanced Elastomer Systems. |
EU 2003/11/EC; RoHS Compliant |