MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Misumi DC53 JIS Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Cold Work Steel; Mold Steel

Material Notes: General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster than D2 and A2. About the same strength as D2 Tool Steel after low-temperature tempering.

Information provided by MISUMI Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 58 - 6358 - 63
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.2 µm/m-°C
@Temperature 20.0 - 100 °C
6.78 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 23.8 W/m-K165 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 180 - 200 °C356 - 392 °FTempered and air cooled
 1020 - 1050 °C1870 - 1920 °FHardened then air cooled

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
International Mold Steel DC53 General-Purpose Cold Work Die and Mold Steel
Bohler-Uddeholm AISI D2 Cold Work Tool Steel
Bohler-Uddeholm BÖHLER W302 ISOBLOC® H13 hot work tool steel
Carpenter S7 Alloy Tool Steel (AISI S7)
Latrobe LSS™ D2 Tool Steel (ASTM D2)

NMISUM951 / 178116

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.