MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 328.0-T6, Sand Cast
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Aluminum Casting Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Key Words: Aluminium 328.0-F; UNS A03280; AA328.0-T6. Comparable to LM27-T6; Al328.0-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.70 g/cc0.0975 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 65 - 9565 - 95AA; Typical; 500 g load; 10 mm ball
Hardness, Knoop 103103Estimated from Brinell Hardness.
Hardness, Rockwell B 4949Estimated from Brinell Hardness.
Hardness, Vickers 9090Estimated from Brinell Hardness.
Tensile Strength, Ultimate >= 234 MPa>= 34000 psiAA
Tensile Strength, Yield >= 145 MPa
@Strain 0.2 %
>= 21000 psi
@Strain 0.2 %
AA
Elongation at Break >= 1.0 %>= 1.0 %AA; in 2 in. (50 mm) or 4D
Tensile Modulus 73.0 GPa10600 ksiEstimated from 360.0
Poissons Ratio 0.330.33Estimated from 360.0
Machinability 50 %50 %0-100 Scale (100=best)
Shear Modulus 27.4 GPa3970 ksiCalculated
Shear Strength 143 MPa20700 psiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000570 ohm-cm0.00000570 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 389 J/g167 BTU/lbTypical for cast aluminum
CTE, linear  21.4 µm/m-°C
@Temperature 20.0 - 100 °C
11.9 µin/in-°F
@Temperature 68.0 - 212 °F
 23.2 µm/m-°C
@Temperature 20.0 - 300 °C
12.9 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.963 J/g-°C0.230 BTU/lb-°FTypical for cast aluminum
Thermal Conductivity 121 W/m-K840 BTU-in/hr-ft²-°F
Melting Point 552 - 596 °C1030 - 1100 °F
Solidus 552 °C1030 °F
Liquidus 596 °C1100 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 86 %86 %As remainder
Chromium, Cr 0.35 %0.35 %
Copper, Cu 1.0 - 2.0 %1.0 - 2.0 %
Iron, Fe 1.0 %1.0 %
Magnesium, Mg 0.20 - 0.60 %0.20 - 0.60 %
Manganese, Mn 0.20 - 0.60 %0.20 - 0.60 %
Nickel, Ni 0.25 %0.25 %
Silicon, Si 7.5 - 8.5 %7.5 - 8.5 %
Titanium, Ti 0.25 %0.25 %
Zinc, Zn 1.5 %1.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum A206.0-T7 Casting Alloy
Aluminum 201.0-T7, Sand Cast
Aluminum 328.0-F, Sand Cast
Aluminum 355.0-T61, Cast
Overview of materials for 3000 Series Aluminum Alloy

MAC3280T6 / 9873

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.