MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Clariant Polyamide 12 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Clariant Polyamide 12 3D printer filament uses a good flowing Polyamide 12. Polyamide 12 is often desired due to its better moisture resistance compared to Polyamide 6. Clariant Polyamide 12 contains a Renol® masterbatch using Clariant Hostanox® P-EPQ® and Nylostab® S-EED®.

General properties:

  • Semi-crystalline thermoplastic
  • Strong and tough engineering thermoplastic
  • High impact strength

Information provided by Clariant.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.18 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPa50 mm/min, Injection Molded; ISO 527
Tensile Strength, Yield 45.0 MPa50 mm/min, Injection Molded; ISO 527
Elongation at Break >= 50 %50 mm/min, Injection Molded; ISO 527
 
Thermal PropertiesOriginal ValueComments
Melting Point 178 °CDSC 10°C/min; ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 115 °CInjection Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 45.0 °CInjection Molded; ISO 75
 
Processing PropertiesOriginal ValueComments
Processing Temperature 190 - 230 °CPrint Temperature
 
Descriptive Properties
Printing Bed AdhesionDirectly on glass, polyimide film, or PEI surface
Printing Bed Temperature70°C Ideal
Printing Fan SettingMedium to High
Printing Speed20 - 40 mm/s
Standard ColorsWhite, Black, Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin
Chevron Phillips Marlex® D139FK Metallocene Linear Low Density Polyethylene, Blown Film
Clariant Black Polyamide 6 3D Printer Filament
Clariant Black Polycarbonate 3D Printer Filament
Corbion Purac Blend B High Heat, High Modulus Homopolymer PLA

PCLAR00001 / 230593

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.