MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Clariant Black Polyamide 6 3D Printer Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Clariant polyamide 6 3D printer filament is made of a good flowing Polyamide 6 that results in high performance 3D printed parts. Clariant Hostanox® P-EPQ® and Nylostab® S-EED® are added via a Renol® masterbatch to improve resistance to thermo-oxidative degradation and minimize yellowing due to ultraviolet radiation

General properties:

  • Semi-crystalline thermoplastic
  • High impact strength
  • High stiffness
  • Outstanding wear resistance
  • Good coefficient of friction
  • Very good temperature resistance

Information provided by Clariant.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.141 g/cc0.04122 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 78.0 MPa11300 psi50 mm/min, Injection Molded; ISO 527
Elongation at Break 20 %20 %50 mm/min, Injection Molded; ISO 527
Flexural Strength 101 MPa14600 psiInjection Molded; ISO 178
Flexural Modulus 2.48 GPa360 ksiInjection Molded; ISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 221 °C430 °FDSC 10°C/min (Natural Color); ISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 165 °C329 °FInjection Molded; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C136 °FInjection Molded; ISO 75
 
Processing PropertiesMetricEnglishComments
Processing Temperature 250 - 280 °C482 - 536 °FPrint Temperature
 
Descriptive Properties
Printing Bed AdhesionDirectly on glass or polyimide film
 PEI surfacewith thin coat of PVP adhesive
Printing Bed Temperature70°C Ideal
Printing Fan SettingMedium to High
Printing Speed20 - 50 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin
Clariant Black Polycarbonate 3D Printer Filament
Clariant Polyamide 12 3D Printer Filament
A. Schulman CP851 High Flow, Injection Molding Grade
Chevron Phillips Marlex® 7109DL LLDPE Blown Film Resin

PCLAR00004 / 230596

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.