MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celcon® LM90 Acetal Copolymer (Capable of being Laser Marked)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Unreinforced

Material Notes: Description: Celcon LM90 is a 9.0 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Celcon LM90 can be laser marked with barcodes, ID numbers and designs.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183 & ASTM D792
Linear Mold Shrinkage 0.022 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 64.0 MPa50 mm/min; ISO 527-2/1A
Flexural Modulus 2.77 GPaISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 105 °CISO 75-1, -2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 199 °C
Mold Temperature 77.0 - 93.0 °C
Drying Temperature 180 °F
Dry Time 3 hour
Injection Pressure 11000 - 16000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hostaform® LM90 POM, Specialty
Celanese Celcon® LM90Z POM, Specialty
Celanese Celcon® M90™ POM, Unfilled
Americhem Engineered Compounds ColorFast® FRA205 ABS
Celanese Celcon® M90-07 POM, Color Concentrate

PHCW17 / 45958

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.