System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Americhem Engineered Compounds ColorFast® FRA205 ABS
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Material Notes:
Flame-retarded V0, high gloss ABS with superior UV stability
All information provided by LTL Color Compounders, Inc. LTL was acquired by Americhem in 2014.
Key Words:
ABS
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.28
g/cc
1.28
g/cc
ASTM D792
Linear Mold Shrinkage
0.0030
-
0.0060
cm/cm
0.0030
-
0.0060
in/in
0.125 in.; ASTM D955
Melt Flow
11
g/10 min
@Load 3.80 kg,
Temperature 230 °C
11
g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
102
102
ASTM D785
Tensile Strength, Yield
38.6
MPa
5600
psi
2.0 in/min; ASTM D638
Elongation at Break
12 %
12 %
2.0 in/min; ASTM D638
Flexural Strength
57.9
MPa
8400
psi
2.0 in/min; ASTM D790
Flexural Modulus
2.34
GPa
340
ksi
2.0 in/min; ASTM D790
Izod Impact, Notched
2.14
J/cm
@Temperature 22.8 °C
4.00
ft-lb/in
@Temperature 73.0 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
72.8
°C
163
°F
Unannealed (0.250"); ASTM D648
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
171
-
182
°C
340
-
360
°F
Middle Barrel Temperature
199
-
210
°C
390
-
410
°F
Front Barrel Temperature
210
-
221
°C
410
-
430
°F
Nozzle Temperature
193
-
221
°C
380
-
430
°F
Melt Temperature
193
-
232
°C
380
-
450
°F
Mold Temperature
71.1
-
82.2
°C
160
-
180
°F
Drying Temperature
71.1
-
82.2
°C
160
-
180
°F
Dry Time
3
-
4
hour
3
-
4
hour
nominal; maximum drying time of 8 hours
Back Pressure
0.345
-
0.689
MPa
50.0
-
100
psi
Shot Size
50 - 70 %
50 - 70 %
Vent Depth
0.00381
-
0.00508
cm
0.00150
-
0.00200
in
Screw Speed
30
-
60
rpm
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Celanese Celcon® LM90 Acetal Copolymer (Capable of being Laser Marked)
LATI LASTILAC ARUV-V0 Acrylonitrile Butadiene Styrene (ABS) (UL94 V-0 5V)
Celanese SO.F.TER Abistir® 7120/V0-UV ABS
Celanese SO.F.TER Abifor® 7145/V0-UV Self Extinguishing ABS, Flame Resistant
PLTLC016 / 104401
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.