MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® CHIPBONDER® 3615 High Adhesion, Syringe Dispense
Categories: Polymer; Adhesive; Thermoset

Material Notes:
Surface Mount Adhesives
Loctite® Chipbonder® Surface Mount Adhesives (SMAs) maintain component positioning during wave solder and solder reflow processes. Loctite offers a variety of application techniques including syringe dispense, stencil print and pin transfer.

Loctite® syringe dispense products provide good performance for electronics assembly:

  • High Speed Dispense
  • Low Temperature Cure
  • Products for difficult-to-bond substrates


Loctite® 3615 CHIPBONDER® High Adhesion, Syringe Dispense
Formulated specifically for hard to bond components. Low moisture pick up. Ideal for Archimedes and piston pump dispense systems.

Peaked dot profile.

Process Method:

  • Medium speed
  • Syringe dispensing
  • 18,000 DPH capable

Storage (Protect from heat): 40°F (+/-5°F) or 5°C (+/-3°C)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 90.0 sec
@Temperature 150 °C
Shelf Life 6.00 MonthFrom date of manufacture
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Loctite® 414 General Purpose Ethyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® Durabond® E-60HP Epoxy Adhesive
Henkel Loctite® CHIPBONDER® 3609 Syringe Dispense
Henkel Loctite® 415 General Purpose Methyl Cyanoacrylate Bonding Adhesive
Henkel Loctite® 410 Toughened Ethyl Cyanoacrylate Bonding Adhesive

PLOCT208 / 51944

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.