MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Mix ratio 2 to 1 by volume.

TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications where outstanding shock and peel resistance are required. TIGA 159 LV-UV can be gelled to a tack free, non-flow state with a few seconds of exposure to moderate UV light and then fully cured at room temperature or rapidly at elevated temperatures. The fully cured system develops strong, tough, high performance bonds to metals, ceramics, phenolics, polyesters, epoxies, urethanes and many other plastics. It is a durable, electrically insulating adhesive which provides good resistance to gases, vapors, petroleum solvents, fuels, salt solutions, mild acids and alkalis.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/cc
Viscosity  2000 cP
@Temperature 25.0 °C
2000 cP
@Temperature 77.0 °F
Of resin
 7500 cP
@Temperature 25.0 °C
7500 cP
@Temperature 77.0 °F
Of hardener
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4040
Flexural Strength 37.9 MPa5500 psi
Adhesive Bond Strength 22.1 MPa3200 psiAl/Al
Izod Impact, Notched 2.14 J/cm4.00 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 16.1 kV/mm410 kV/in
Dissipation Factor 0.038
@Frequency 100000 Hz
0.038
@Frequency 100000 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 120 - 180 min
@Temperature 25.0 °C
120 - 180 min
@Temperature 77.0 °F
100 gm mass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trelleborg Emerson & Cuming Eccobond® G 909 One-Component Fast Cure Epoxy Adhesive
Tra-Con Tra-Bond 832-5 Flexible Epoxy
Resinlab® EP1121 Black Electronic Grade Epoxy Encapsulant
Resinlab® EP1112NC Black Electronic Grade Epoxy Encapsulant
Henkel Loctite® Durabond® U-10FL Urethane Adhesive

PRESINT653 / 65537

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.