MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
C.O.I.M. FILCO® 657 Unsaturated Polyester Powder Resin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Description: Unsaturated Polyester Powder Resin
General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.
Applications: Filco 657 is used as a binder in both chopped and continuous fiber glass products for the production of thermosetting glass/resin composites in low pressure molding in RTM injection or in reinforcement of polyurethane foams.
Filco 657 has good melting capacity and high heat reactivity. Drying temperatures between 170°C and 200°C at 40 - 70 seconds are recommended for application. After cross-linking, Filco 656 becomes insoluble (in styrene) and acquires its binding power.
Note: According to the customer, the peroxide content may be modified.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesOriginal ValueComments
Acid Value 35 - 45mgKOH/g
 
Thermal PropertiesOriginal ValueComments
Melting Point 103 - 107 °C
 
Descriptive Properties
AppearanceWhite Crystalline Powder
Dibenzoyl Peroxide Content1.0 ± 0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
C.O.I.M. FILCO® 656 Unsaturated Polyester Powder Resin
C.O.I.M. FILCO® 362 Film Former for Glass Fiber Sizes
C.O.I.M. FILCO® 350 Non Ionic Unsaturated Polyester Polymer Emulsion for Glass Fiber Sizing
C.O.I.M. FILCO® 352 Unsaturated Bisphenolic Polyester Polymer for Glass Fiber Sizing
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes

PCOIM113 / 28716

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.