MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

C.O.I.M. FILCO® 656 Unsaturated Polyester Powder Resin
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic

Material Notes: Description: Unsaturated Polyester Powder Resin
General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.
Applications: Filco 656 is used as a binder in both chopped and continuous fiber glass products for the production of thermosetting glass/resin composites in low pressure molding in RTM injection or in reinforcement of polyurethane foams.
Filco 656 has good melting capacity and high heat reactivity. Drying temperatures between 170°C and 200°C at 40 - 70 seconds are recommended for application. After cross-linking, Filco 656 becomes insoluble (in styrene) and acquires its binding power.
Note: According to the customer, the peroxide content may be modified.
Information provided by P.A.T. Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Chemical PropertiesMetricEnglishComments
Acid Value 35 - 4535 - 45mgKOH/g
 
Thermal PropertiesMetricEnglishComments
Melting Point 103 - 107 °C217 - 225 °F
 
Descriptive Properties
AppearanceWhite Crystalline Powder
Dibenzoyl Peroxide Content0.8 ± 0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. FILCO® 657 Unsaturated Polyester Powder Resin
Menzolit Menzolit® BMC 0160 Unsaturated Polyester UP
Bakelite® UP 802 Unsaturated Polyester Resin, High Surface Quality, Low Shrinkage, High Arc Resistance
Bakelite® UP 3415 Unsaturated Polyester Resin, Low Shrinkage, High Arc Resistance, UL Listed, High Mechanical Strength
C.O.I.M. FILCO® 350 Non Ionic Unsaturated Polyester Polymer Emulsion for Glass Fiber Sizing

PCOIM112 / 28715

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.