MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics CHO-THERM® 1680 Thermally Conductive Insulators for Surface Mount Applications
Categories: Polymer; Thermoset; Silicone

Material Notes: CHO-THERM® 1680 thermal interface insulators efficiently transfer heat away from mounted components with out the need for clamping force. These pads have a high tack, pressure-sensitive adhesive on one or both sides. This configuration is optimized for mounting multichip modules and other surface mount components to PBCs. CHO-THERM® 1680 thermal pads are composed of a polyimide film beneath a layer of boron nitride-filled silicone, with adhesive on one or both sides. The 0.001 in. thick polyimide film offers excellent resistance to cut-through. The film is coated on one side with a resilient boron nitride-filled silicone, providing an effective thermal path. The adhesive bonds components to provide good heat transfer under low mounting pressures. This is especially useful in applications such as hybrid, ceramic, and flat packages.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Thickness 180 microns7.09 milASTM D374
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 1010ASTM D2240
Tensile Strength 27.6 MPa4000 psiASTM D412
Elongation at Break 25 %25 %ASTM D412
Tear Strength 35.1 kN/m200 pliASTM D642
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Breakdown 6000 V6000 VASTM D149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.650 W/m-K4.51 BTU-in/hr-ft²-°FASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Descriptive Properties
BinderSilicone
CarrierPolyimide
ColorWhite/Gold
FillerBoron Nitride

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 816H02 Thermally Conductive Electrically Insulating Compound
Premix Thermoplastics PRETHERM TPE 1050 Thermoplastic Elastomer, Boron Nitride / SEBS compound

PCHOME249 / 130959

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.