MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
China-Yixing Longly Refractories 99 Alumina Ceramic Tube & Rod
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: LONGLY's alumina ceramic tubes and rods (the tolerances of +/- 0.02mm could be reached by mechanical or electronic finishing or mirror surface finishing) have high hardness, wear resistance, insulation and high temperature resistance. Alumina ceramic tubes are mainly applicable to the material conveying with wear resistant and heavy scouring resistant demands, such as material conveying pipelines for coal-fired power generation, metallurgical and geological industries. Meanwhile they can be used as fuse insulating tube on the electric and electronic appliances. Alumina ceramic rods are used as resistor's ceramic matrix and ceramic top pillar on two-metal thermostat.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.80 - 3.90 g/cc
Water Absorption <= 0.0020 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 9.0
Flexural Strength >= 580 MPacold bending
Compressive Strength >= 560 MPaAmbient
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+16 ohm-cm
@Temperature 100 °C
Dielectric Strength 15.2 - 16.7 kV/mmDC Breakdown Strength
 19.0 kV/mmInsulating Strength
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.80 - 8.30 µm/m-°C
@Temperature 25.0 - 800 °C
Thermal Conductivity 33.0 W/m-K
Maximum Service Temperature, Air >= 1600 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 98.2 - 99.5 %
 
Descriptive Properties
Refractoriness (°C)>2030

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Ceramic Lining Plates and Pieces

CYXLR021 / 99323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.