MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

China-Yixing Longly Refractories Microcrystal Wear-Resistant Alumina Ceramic Lining Plates and Pieces
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: LONGLY's wear-resistant alumina ceramic lining plates and pieces are special alumina ceramics produced on the basis of Al2O3 by dry pressing with rare metal oxide as solvent, sintered under a high temperature of 1700°C. They could endure various wear resistant demands according to specific condition.

Characteristics: With a Rockwell hardness of HRA80-90 (just inferior to diamond), its wear resistance is far superior to wear-resistant steel and stainless steel, which is 266 times that of manganese steel and 171.5 times that of high chromium cast iron. The bulk density is 3.6 g/cc, just a half of steel, which could reduce equipment load. These alumina ceramic lining plates or pieces can be stuck to the interior wall of the equipment by strong heat resistant adhesive.

Applications: As for those mechanical equipment of heavy wearing used in conveying system for coal and materials, pulverizing system, ash and dust removing system of enterprises related to thermal power, steel, smelting, machinery, coal, mine, chemical, cement and port, different types of products could be chosen as per specific need.

Information Provided by China Yixing Longly Refractories Co. Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.50 - 3.60 g/cc0.126 - 0.130 lb/in³
Water Absorption <= 0.020 %<= 0.020 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 9.09.0
Compressive Strength 1700 - 2200 MPa247000 - 319000 psiCrushing Strength
Fracture Toughness 6.00 - 6.80 MPa-m½5.46 - 6.19 ksi-in½
 
Component Elements PropertiesMetricEnglishComments
Al2O3 91 - 95.8 %91 - 95.8 %
Fe2O3 0.20 - 0.25 %0.20 - 0.25 %
 
Descriptive Properties
Wear Loss (%)0.10-0.15

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A662 Carbon Steel, Grade A
China-Yixing Longly Refractories 99 Alumina Ceramic Tube & Rod
Thermal Ceramics Superwool 607 Max Pyro-Fold and Pyro-Stack Modules
Thermal Ceramics Superwool 607 Pyro-Fold and Pyro-Stack Modules
ASTM A662 Carbon Steel, Grade C

CYXLR023 / 99325

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.