MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Mix ratio 2 to 1 by volume.

UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy based polymer is designed to gel with exposure to UV light followed by complete cure by internal chemical cross-link, with or without UV exposure. UV-MX 2240’s ability to “dark-cure” via conventional amine cure cross-linking makes it ideal for those applications that require the on-line speed of a UV cure and the versatility of a conventional two-part epoxy cure.

Applications:

Recommended for laminating, bonding and sealing applications of glass products where excellent wetting and outstanding impact strength is required. Electronic-Opto: Back filling of connectors, LED potting, glass touch screens.

Processing:

UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometers.

Information provided by Resin Technology Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 g/cc1.05 g/cc
Viscosity 300 - 500 cP
@Temperature 25.0 °C
300 - 500 cP
@Temperature 77.0 °F
Mixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545
Tensile Strength at Break >= 13.8 MPa>= 2000 psiCured
Elongation at Break 20 %20 %Cured
Compressive Strength >= 34.5 MPa>= 5000 psiCured
Shear Strength >= 6.89 MPa>= 1000 psiCured, lap, Al/Al, at 25°C
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.7 kV/mm>= 400 kV/inCured
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
Cured
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 100 °C
0.500 hour
@Temperature 212 °F
 120 min
@Temperature 65.0 °C
2.00 hour
@Temperature 149 °F
 2880 - 10100 min
@Temperature 23.0 °C
48.0 - 168 hour
@Temperature 73.4 °F
Pot Life 30.0 min
@Temperature 25.0 °C
30.0 min
@Temperature 77.0 °F
Gel Time 0.167 - 0.333 min0.167 - 0.333 min400 watt UV
 
Descriptive Properties
ColorWater white

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Adhesive
Resin Technology Group UV MX-2231 Hybrid, UV Curing, Thermal-Cure, Micro-Electronic Encapsulant
Dymax 9-20493 Voil Coil Assembly Disk Drive Adhesive
Henkel Loctite® 3761 Acrylic Light Cure Adhesive
Henkel Loctite® 3103 Acrylic Light Cure Adhesive

PRESINT656 / 65540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.