MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil NTX™ NTX 104 Super Strength Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: NTX super strength hexene blown film resins are designed for applications requiring exceptional strength for maximum downgauging potential. Key property improvements are significantly superior impact and tear strength. NTX resins are formulated with various additive packages for use in all high performance film applications.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.917 g/ccASTM D1505
Thickness 1.00 mil
Melt Flow 0.90 g/10 minASTM D1238
Antiblock Level 6500 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 1500 psiASTM D882
Film Tensile Strength at Yield, TD 1500 psiASTM D882
Film Elongation at Break, MD 565 %ASTM D882
Film Elongation at Break, TD 775 %ASTM D882
Elmendorf Tear Strength, MD 430 g/milASTM D1922
Elmendorf Tear Strength, TD 750 g/milASTM D1922
Dart Drop 480 g/milASTM D1709
Film Tensile Strength at Break, MD 8000 psiASTM D882
Film Tensile Strength at Break, TD 5800 psiASTM D882
1% Secant Modulus, MD 28000 psiASTM D882
1% Secant Modulus, TD 30000 psiASTM D882
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil NTX™ NTX 150 Super Strength Film Resin
ExxonMobil NTX™ NTX 141 Super Strength Film Resin
ExxonMobil NTX™ NTX 101 Super Strength Film Resin
ExxonMobil NTX™ NTX 095 Super Strength Film Resin
ExxonMobil C4LL 1018.32 Linear Low Density Polyethylene Resin

PEXB245 / 37550

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.