Product Description: ExxonMobil™ C4LL 1018.32 is an ethylene 1-butene linear low density polyethylene resin. Films made from ExxonMobil™ C4LL 1018.32 resin have very good tensile and toughness properties. Availability: Latin America and North America Additive: - Antiblock: No
- Slip: No
- Processing Aid: No
- Thermal Stabilizer: Yes
Applications: - Cast Film
- Cast Stretch Film
- Industrial Liners
- Liners
- Produce Bags
- Refuse Bags
- Trash Bags
Information provided by ExxonMobil |