Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties. Availability: Latin America, North America and South America Additive: - Antiblock: No
- Slip: No
- Processing Aid: No
- Thermal Stabilizer: Yes
Applications: - Cast Film
- Cast Stretch Film
- Industrial Liners
- Liners
- Produce Bags
- Refuse Bags
- Trash Bags
Information provided by ExxonMobil |