MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solvay DAPCO™ 3008 Low Density, Self-Extinguishing Honeycomb Filler
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: DAPCO™ 3008 is a two-component, self-extinguishing epoxy filler.

Features & Benefits:

  • Cure at room temperature
  • Excellent adhesion to metal and wood
  • Very low water absorption
  • Good chemical resistance, especially to aircraft fluids
  • Can be nailed, threaded, countersunk, drilled, cut, etc. without cracking or chipping
  • 100% solids
  • FAR 25.853
Applications: DAPCO 3008 is commonly used for potting, stiffening and edge filling in honeycomb core.

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.449 - 0.513 g/cc0.0162 - 0.0185 lb/in³
Solids Content 100 %100 %Part A
 100 %100 %Part B
 100 %100 %Mixed
Water Absorption 0.40 %
@Time 86400 sec
0.40 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D224
Flexural Modulus 1.38 GPa200 ksi
Compressive Strength 20.7 MPa3000 psi
 
Descriptive Properties
ColorLight yellowMixed
 WhitePart A
 YellowPart B
Mix Ratio100:35Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elantas EN-2523 (Conap) Potting and Encapsulation Adhesive
Hexcel® HexWeb® CR III 1/8-5056-.001 Corrosion Resistant Specification Grade Aluminum Honeycomb
Solvay BR® 680-3 Polyimide Film Adhesive
Ultracor® UCF-51-3/8-2.0 Honeycomb Core Material
Solvay DAPCO™ 3041FR Paste Adhesive

PCYTED015 / 180317

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.