MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elantas EN-2523 (Conap) Potting and Encapsulation Adhesive
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes:
Polyurethane Potting and Encapsulating Systems
Conathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many specific potting and encapsulating applications such as modules, strain-sensitive components, transformers, and coils. All 2500 series systems exhibit excellent performance when exposed to adverse environments and temperature ranges between -55°C and +130°C.

Cytec (Conap) EN-2523 Potting and Encapsulation Adhesive

  • Passes Thermal Shock Test (10 Cycles, -65°C to 130°C)
  • Non-Nutrient Fungus Resistance (MIL-STD-810B)
  • Mix Ratio: 20/100 (by Weight)

Information provided by Cytec, subsequently acquired by Elantas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.44 g/cc0.0520 lb/in³Cured
Water Absorption 0.14 %0.14 %24 hours
Water Absorption at Saturation 0.0045 %0.0045 %30 Days
Viscosity 2800 cP
@Temperature 25.0 °C
2800 cP
@Temperature 77.0 °F
Linear Mold Shrinkage 0.0059 cm/cm0.0059 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 50 - 5550 - 55
Tensile Strength, Ultimate 11.0 MPa1600 psi
Elongation at Break 50 %50 %
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 3.40e+13 ohm-cm<= 3.40e+13 ohm-cm
Surface Resistance 1.50e+13 ohm1.50e+13 ohm
Dielectric Constant 4.1
@Frequency 1000 Hz
4.1
@Frequency 1000 Hz
Dielectric Strength 24.8 kV/mm
@Thickness 1.59 mm
630 kV/in
@Thickness 0.0625 in
Dissipation Factor 0.049
@Frequency 1000 Hz
0.049
@Frequency 1000 Hz
Arc Resistance >= 120 sec>= 120 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 150 µm/m-°C
@Temperature 20.0 °C
83.3 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 0.188 W/m-K1.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C266 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  240 min
@Temperature 100 °C
4.00 hour
@Temperature 212 °F
 360 min
@Temperature 60.0 °C
6.00 hour
@Temperature 140 °F
 10080 min
@Temperature 25.0 °C
168.0 hour
@Temperature 77.0 °F
Pot Life 45.0 - 50.0 min
@Temperature 25.0 °C
45.0 - 50.0 min
@Temperature 77.0 °F
1 lbm
 
Descriptive Properties
ColorTan or Black

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay BR® 680-3 Polyimide Film Adhesive
Solvay DAPCO™ 3041FR Paste Adhesive
Solvay DAPCO™ 3008 Low Density, Self-Extinguishing Honeycomb Filler
Solvay BR® 4535A Paste Adhesive
Solvay A6000 ETFE Fluoropolymer Film

PCYTEC19 / 29251

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.