MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Sumitomo Bakelite Durez® 13355 Phenolic Novolac
Categories: Polymer; Thermoset; Phenolic

Material Notes: Durez® 13355 is a finely powdered, thermosetting, oil modified phenolic resin of the two-step type. It has a medium cure and a medium-hard set. It can be used as reinforcing resin for synthetic rubbers in tire and technical rubber manufacturing.

Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Mesh Size 200 Mesh200 MeshScreen Percent: 1; DCT 7-200
 
Thermal PropertiesMetricEnglishComments
Melting Point 74.0 °C165 °FShrink; DCT 11S
 
Processing PropertiesMetricEnglishComments
Cure Time 0.467 min
@Treatment Temp. 165 °C
0.00778 hour
@Treatment Temp. 329 °F
DCT 162
 
Descriptive Properties
AppearanceCream Colored Powder
Inclined Plate Flow; 0.2g, 125°C, mm60DCT 351

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sumitomo Bakelite Durez® 13349 Phenolic Novolac
Sumitomo Bakelite Durez® 152 Phenolic, Injection Grade
Sumitomo Bakelite North America RX® 853G Fiberglass Reinforced Phenolic Novolac
Sumitomo Bakelite Durez® 32633 Glass Filled Phenolic, Injection Grade
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC

PSUMIT222 / 194027

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.