Durez® 13355 is a finely powdered, thermosetting, oil modified phenolic resin of the two-step type. It has a medium cure and a medium-hard set. It can be used as reinforcing resin for synthetic rubbers in tire and technical rubber manufacturing.Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |