MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay SIPOMER® PAM-4000 Ethylmethacrylate Phosphate; Alkyl Methacrylate Phosphate
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Sipomer PAM-4000 incorporated into acrylic or styrene acrylic systems improves adhesion to metallic substrates. It also enhances properties such as polymer stability and gloss. This monomer has been used mainly in specialty purpose coatings, including industrial maintenance, OEM, as well as high performance structural adhesives.

Chemical Name: ETHYLMETHACRYLATE PHOSPHATE; ALKYL METHACRYLATE PHOSPHATE

CAS: 52628-03-2, 7664-38-2, 868-77-9

Available in: Asia Pacific, Europe, Latin America and North America

Applications: SIPOMER ® PAM-4000 incorporated into acrylic or styrene acrylic systems improves adhesion to metallic substrates. It also enhances properties such as polymer stability and gloss. This monomer has been used mainly in specialty purpose coatings, including industrial maintenance, OEM, as well as high performance structural adhesives.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH <= 1.0<= 1.0
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 171 - 187171 - 187[mg KOH/g], #1; RP-0427
 266 - 296266 - 296[mg KOH/g], #2; RP-0427
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.25 %<= 0.25 %PRC11006
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceClear, Colorless to Pale Yellow Liquid
Color<300APHA, RPC11004
CompositionMEHQ250-600 ppm, RP-1408
 Phosphoric Acid<4%, RP-0427
OdorMild Acrylic Odor

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay SIPOMER® PAM-100 Phosphate Esters of Polyethylene Glycol Monomethacrylate
Solvay SIPOMER® WAM II Composition Based On Methacrylamidoethyl Ethylene Urea
Solvay SIPOMER® WAM Allyl / Ureido Monomer
Solvay SIPOMER® SEM 25 Polyalkoxyl Polyarylphenol Ethylenic Methacrylate
Solvay SIPOMER® PAM-300 Phosphate Esters of Ppg Monoacrylate

WRHOD508 / 137739

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.