MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Raschig Group SURAPLAST 54 UPA
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS

Material Notes: Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (WEEE) and 2006/122 (PFOS).

Processing: Injection molding

Primary application: Contact terminals, relays, circuit breakers

Information provided by the Raschig Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 - 2.10 g/cc1.90 - 2.10 g/ccISO 1183
Apparent Bulk Density 0.700 - 0.800 g/cc0.0253 - 0.0289 lb/in³ISO 60
Water Absorption <= 0.50 %
@Temperature 23.0 °C,
Time 86400 sec
<= 0.50 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inCompression; ISO 2577
 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inInjection; ISO 2257
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 35.0 - 60.0 MPa5080 - 8700 psiCompression; ISO 527
 40.0 - 70.0 MPa5800 - 10200 psiInjection; ISO 527
Modulus of Elasticity 9.00 - 11.0 GPa1310 - 1600 ksiInjection and Compression; ISO 527
Flexural Strength 80.0 - 100 MPa11600 - 14500 psiCompression; ISO 178
 100 - 120 MPa14500 - 17400 psiInjection; ISO 178
Flexural Modulus 10.0 - 13.0 GPa1450 - 1890 ksiCompression; ISO 178
 13.0 - 16.0 GPa1890 - 2320 ksiInjection; ISO 178
Compressive Strength 150 - 200 MPa21800 - 29000 psiISO 604
Charpy Impact Unnotched  0.500 - 1.00 J/cm²
@Temperature 23.0 °C
2.38 - 4.76 ft-lb/in²
@Temperature 73.4 °F
Compression; ISO 179 1eU
 0.800 - 1.10 J/cm²
@Temperature 23.0 °C
3.81 - 5.24 ft-lb/in²
@Temperature 73.4 °F
Injection; ISO 179/ 1eU
Charpy Impact, Notched  0.250 - 0.350 J/cm²
@Temperature 23.0 °C
1.19 - 1.67 ft-lb/in²
@Temperature 73.4 °F
Compression; ISO 179 1eA
 0.350 - 0.500 J/cm²
@Temperature 23.0 °C
1.67 - 2.38 ft-lb/in²
@Temperature 73.4 °F
Injection; ISO 179/ 1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 - 1.00e+15 ohm-cm1.00e+14 - 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+13 - 1.00e+14 ohm1.00e+13 - 1.00e+14 ohmIEC 60093
Dielectric Constant  4.0 - 5.0
@Frequency 1e+6 Hz
4.0 - 5.0
@Frequency 1e+6 Hz
IEC 60250
 5.0 - 6.0
@Frequency 100 Hz
5.0 - 6.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 0.984 - 1.38 kV/mm25.0 - 35.0 kV/inIEC 60243-1
Dissipation Factor  0.010 - 0.030
@Frequency 100 Hz
0.010 - 0.030
@Frequency 100 Hz
IEC 60250
 0.010 - 0.030
@Frequency 1e+6 Hz
0.010 - 0.030
@Frequency 1e+6 Hz
IEC 60250
Arc Resistance >= 180 sec>= 180 secASTM D495
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.0 - 20.0 µm/m-°C
@Temperature 50.0 - 100 °C
5.56 - 11.1 µin/in-°F
@Temperature 122 - 212 °F
ISO 11359-2
Thermal Conductivity 0.900 - 1.10 W/m-K6.25 - 7.63 BTU-in/hr-ft²-°FASTM E1461
Maximum Service Temperature, Air 170 °C338 °F20,000 h; IEC 60216/T1
 210 °C410 °F< 50 h; IEC 60216/T1
Deflection Temperature at 8.0 MPa >= 200 °C>= 392 °FInjection and Compression; ISO 75-C
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
Shrinkage <= 0.10 %
@Temperature 110 °C,
Time 605000 sec
<= 0.10 %
@Temperature 230 °F,
Time 168 hour
Post shrinkage; ISO 2577
 
Processing PropertiesMetricEnglishComments
Mold Temperature 165 - 180 °C329 - 356 °F
Shelf Life 6.00 Month
@Temperature 15.0 - 25.0 °C
6.00 Month
@Temperature 59.0 - 77.0 °F
 
Descriptive Properties
Arc resistance4 StufeASTM D495
Glow wire ignitability test850/1IEC 60695 2-13
Glow-wire flammability test960/1IEC 60695 2-12
Water Absorption<35 mgISO 62; 24h / 23°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoset Polyester Glass SMC
Raschig Group 2567 AMC
Raschig Group RALUPOL® 8602 UP
Raschig Group RALUPOL® 8601 UP
Raschig Group RALUPOL® 4806 UP

PRASCH43 / 65328

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.