MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex Sarlink® TPE ME-2665B BLK9096 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2600 series are super high flow high performance thermoplastic elastomer series, available in BLK, designed for automotive exterior molded applications. Sarlink ME-2665B is a medium hardness, low density, resilient, UV stabilized, super high flow injection molding grade excellent delivering excellent aesthetics with good adhesion to glass with primer.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; Low Density; High Flow; Low Specific Gravity; Medium Hardness; Outstanding Surface Finish; Resilient; UV Resistant

Uses: Automotive Applications; Automotive Exterior Part; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.965 g/ccISO 1183
Viscosity 137 cP
@Shear Rate 206 1/s,
Temperature 200 °C
ASTM D3835
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 62
@Time 5.00 sec
Injection Molded; ISO 868
 64
@Time 1.00 sec
Injection Molded; ISO 868
 62
@Treatment Temp. 130 °C,
Time 5.00 sec
Change in Air, 168 hr; ISO 188
Tensile Strength at Break 1010 psiISO 37
 919 psi
@Treatment Temp. 130 °C,
Time 605000 sec
Change in Air; ISO 188
Elongation at Break 810 %ISO 37
 891 %
@Treatment Temp. 130 °C,
Time 605000 sec
Change in Air; ISO 188
Tear Strength 150 pliISO 34-1
Compression Set 36 %
@Temperature 22.8 °C,
Time 166000 sec
VW PV3307
 73 %
@Temperature 70.0 °C,
Time 166000 sec
VW PV3307
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 338 - 374 °F
Middle Barrel Temperature 347 - 383 °F
Front Barrel Temperature 356 - 401 °F
Nozzle Temperature 356 - 401 °F
Melt Temperature 356 - 401 °F
Mold Temperature 59.0 - 104 °F
Injection Pressure 200 - 1000 psi
Back Pressure 25.0 - 125 psi
Cushion 0.150 - 1.00 in
Screw Speed 50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ1085 / 237576

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.