MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teknor Apex Sarlink® TPE ME-2665B BLK9096 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink ME-2600 series are super high flow high performance thermoplastic elastomer series, available in BLK, designed for automotive exterior molded applications. Sarlink ME-2665B is a medium hardness, low density, resilient, UV stabilized, super high flow injection molding grade excellent delivering excellent aesthetics with good adhesion to glass with primer.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Processability; Low Density; High Flow; Low Specific Gravity; Medium Hardness; Outstanding Surface Finish; Resilient; UV Resistant

Uses: Automotive Applications; Automotive Exterior Part; Automotive Window Encapsulation; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.965 g/cc0.0349 lb/in³ISO 1183
Viscosity 137 cP
@Shear Rate 206 1/s,
Temperature 200 °C
137 cP
@Shear Rate 206 1/s,
Temperature 392 °F
ASTM D3835
Melt Flow 40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  62
@Time 5.00 sec
62
@Time 0.00139 hour
Injection Molded; ISO 868
 64
@Time 1.00 sec
64
@Time 0.000278 hour
Injection Molded; ISO 868
 62
@Treatment Temp. 130 °C,
Time 5.00 sec
62
@Treatment Temp. 266 °F,
Time 0.00139 hour
Change in Air, 168 hr; ISO 188
Tensile Strength at Break 6.96 MPa1010 psiISO 37
 6.34 MPa
@Treatment Temp. 130 °C,
Time 605000 sec
919 psi
@Treatment Temp. 266 °F,
Time 168 hour
Change in Air; ISO 188
Elongation at Break 810 %810 %ISO 37
 891 %
@Treatment Temp. 130 °C,
Time 605000 sec
891 %
@Treatment Temp. 266 °F,
Time 168 hour
Change in Air; ISO 188
Tear Strength 26.3 kN/m150 pliISO 34-1
Compression Set  36 %
@Temperature 22.8 °C,
Time 166000 sec
36 %
@Temperature 73.0 °F,
Time 46.0 hour
VW PV3307
 73 %
@Temperature 70.0 °C,
Time 166000 sec
73 %
@Temperature 158 °F,
Time 46.0 hour
VW PV3307
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 170 - 190 °C338 - 374 °F
Middle Barrel Temperature 175 - 195 °C347 - 383 °F
Front Barrel Temperature 180 - 205 °C356 - 401 °F
Nozzle Temperature 180 - 205 °C356 - 401 °F
Melt Temperature 180 - 205 °C356 - 401 °F
Mold Temperature 15.0 - 40.0 °C59.0 - 104 °F
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psi
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1085 / 237576

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.