MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Polyester Grade

Material Notes: Features: Fast cycling, broad temperature performance, and durability

Use: Injection Molding

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
Maximum Moisture Content 0.020
Linear Mold Shrinkage 0.0080 cm/cmflex bar
 0.013 cm/cmdisk
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52 - 58
@Time 5.00 sec
ASTM D2240
Tensile Strength 41.0 MPaASTM D412
Elongation at Break 500 %ASTM D412
100% Modulus 0.0150 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0270 GPa
@Strain 300 %
ASTM D412
Flexural Modulus 23000 psiASTM D790
Tear Strength 240 pliTrouser; ASTM D470
Graves Tear Strength 900 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 34CS-17, 1000g; ASTM D3389 B
Compression Set 37 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM D395
 49 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Melting Point 221 °CDSC
Glass Transition Temp, Tg -30.0 °CDSC
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 210 °CInjection
Middle Barrel Temperature 215 °CInjection
Front Barrel Temperature 224 °CInjection
Nozzle Temperature 229 °CInjection
Melt Temperature 229 °CInjection
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C
Injection Pressure 10000 - 15000 psiInjection
Hold Pressure 5000 - 10000 psiInjection
Back Pressure >= 50.0 psiInjection
Screw Speed 60 - 100 rpmInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane
Envalior Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America)
Lubrizol ESTANE® 58134 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Lubrizol Estane® 2102-75A Thermoplastic Polyurethane Elastomer

PNOVEON023 / 55289

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.