MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Trelleborg Sealing Solutions Turcite® TA Self-Lubricating Thermoplastic Rod
Categories: Polymer; Thermoplastic

Material Notes: Turquoise color. Turcite® TA was developed for general purpose load and speed applications. It exhibits an excellent surface finish when machined. It has exceptional service life and superior chemical resistance.

General Turcite® information: Exhibit excellent wear resistance, durability, and no slip-stick under oscillating motion. Axial-loaded shafts benefit from reduced friction. Uses include transmissions, home appliances, bicycles, food processing equipment, exercise equipment, rotating displays, and caster assemblies.

Information provided by Busak + Shamban, now Trelleborg Sealing Solutions.

Busak+Shamban changed its name to Trelleborg Sealing Solutions in 2007.

Key Words: Busak + Shamban; TI Group; Smiths Group
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.20 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 52.4 MPa
Elongation at Break 15 %
Coefficient of Friction 0.30non-lubricated
K (wear) Factor 43.0 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 0.260 MPa-m/sec
 
Thermal PropertiesOriginal ValueComments
CTE, linear 93.6 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 82.0 °CContinuous
 96.0 °CDeflection Temperature with load unspecified
 107 °CIntermittent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trelleborg Sealing Solutions Turcite® TX Self-Lubricating Thermoplastic Rod
Saint-Gobain Rulon® LR Bearing/Seal PTFE
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Special Metals MONEL® Alloy 400

PSMIT0 / 67853

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.