MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Furan (C4H4O)
Categories: Fluid; Solvent

Key Words: C4H4O
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9514 g/cc
@Temperature 20.0 °C
Viscosity 0.361 cP
@Temperature 25.0 °C
 0.38 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 68.08 g/mol
Vapor Pressure 0.09869 atm
@Temperature -20.0 °C
Extrapolated beyond actual measurements.
 493.373 torr
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 54.281 atm
Critical Temperature 217.08 °C
Critical Density 0.312 g/cc
Critical Molar Volume 218 cm³/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 55.82 J/gEnthalpy of fusion at normal melting point
Heat of Vaporization 398.1 J/gEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 0.960 J/g-°C
@Temperature 25.0 °C
Vapor
Thermal Conductivity 0.126 W/m-K
@Temperature 25.0 °C
Melting Point -85.61 °CAt atmospheric pressure (760 torr)
Boiling Point 31.4 °C
@Pressure 0.101 MPa
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4214
@Temperature 20.0 °C,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.0612
Antoine's Vapor Pressure B Parameter2442.7
Antoine's Vapor Pressure C Parameter-45.41
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)110-00-9
Chemical FormulaC4H4O
Critical Compressibility (Zc)0.294
Dipole moment (p/C.m)2.335E-28
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A389.4
Dynamic Viscosity Parameter B222.7
Henry's Law Constant (atm m3/mol)0.00538
Molar Heat Capacity (298K)65.39 J/mol-K
Molar Heat Capacity of Vapor a Parameter-35.5054
Molar Heat Capacity of Vapor b Parameter0.4318
Molar Heat Capacity of Vapor c Parameter-0.0003452
Molar Heat Capacity of Vapor d Parameter1.074E-07
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number2389

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Latrobe LSS™ D2 Tool Steel (ASTM D2)
Methyl Ethyl Ketone (CH3CH2COCH3; 2-Butanone; MEK)
Shandong Dongyue Shenzhou New Material Co Perfluoropropylenevinylether (PPVE)
Latrobe LSS™ Vertex Tool Steel
Hydrazoic Acid, HN3

VORG022 / 74533

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.