MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Methyl Ethyl Ketone (CH3CH2COCH3; 2-Butanone; MEK)
Categories: Fluid; Solvent

Key Words: CH3CH2COCH3
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.8054 g/cc
@Temperature 20.0 °C
0.02910 lb/in³
@Temperature 68.0 °F
Viscosity  0.405 cP
@Temperature 25.0 °C
0.405 cP
@Temperature 77.0 °F
 0.413 cP
@Temperature 20.0 °C
0.413 cP
@Temperature 68.0 °F
Dynamic Viscosity
Molecular Weight 72.12 g/mol72.12 g/mol
Vapor Pressure  0.099869 bar
@Temperature 20.0 °C
74.908 torr
@Temperature 68.0 °F
 0.1000 bar
@Temperature 21.2 °C
75.00 torr
@Temperature 70.2 °F
Surface Tension 24.6 dynes/cm
@Temperature 20.0 °C
24.6 dynes/cm
@Temperature 68.0 °F
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 42.0699 bar31555.0 torr
Critical Temperature 263.62 °C506.52 °F
Critical Density 0.270 g/cc0.00975 lb/in³
Critical Molar Volume 267 cm³/mol16.3 in³/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 18.51
@Temperature 20.0 °C
18.51
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 116.3 J/g50.05 BTU/lbEnthalpy of fusion at normal melting point
Heat of Vaporization 434 J/g187 BTU/lbEnthalpy of vaporization at normal boiling temperature
Specific Heat Capacity 2.203 J/g-°C0.5265 BTU/lb-°F
 1.402 J/g-°C
@Temperature 25.0 °C
0.3351 BTU/lb-°F
@Temperature 77.0 °F
Vapor
Thermal Conductivity 0.145 W/m-K
@Temperature 25.0 °C
1.01 BTU-in/hr-ft²-°F
@Temperature 77.0 °F
Melting Point -86.64 °C-124.0 °FAt atmospheric pressure (760 torr)
Boiling Point 30.0 °C86.0 °Fat 10 torr
 79.6 °C
@Pressure 0.101 MPa
175 °F
@Pressure 14.7 psi
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3788
@Temperature 20.0 °C,
Wavelength 589.3 nm
1.3788
@Temperature 68.0 °F,
Wavelength 589.3 nm
Na D line
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.5986
Antoine's Vapor Pressure B Parameter3150.42
Antoine's Vapor Pressure C Parameter-36.65
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)78-93-3
Chemical FormulaC4H8O
Critical Compressibility (Zc)0.249
Dipole moment (p/C.m)1.101E-27
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A423.84
Dynamic Viscosity Parameter B231.67
Henry's Law Constant (atm m3/mol)5.59E-05
Molar Heat Capacity (298K)101.143 J/mol-K
Molar Heat Capacity of Vapor a Parameter10.937
Molar Heat Capacity of Vapor b Parameter0.3557
Molar Heat Capacity of Vapor c Parameter-0.0001899
Molar Heat Capacity of Vapor d Parameter3.971E-08
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1193
UV cut-off (nm)330

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 7000 Engineered Fluid
Shandong Dongyue Shenzhou New Material Co Perfluoropropylenevinylether (PPVE)
LG Chemical LGflex TINTM Plasticizer
Methyl Isobutyl Ketone ((CH3)2CHCH2COCH3; MIBK; MIK; Hexone)
AGC Asahiklin AE3000AT Solvent

VORG031 / 74542

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.