MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
EDRO UltraChem® ESR #16 Precipitation Hardening Stainless Mold Steel
Categories: Metal; Ferrous Metal; Stainless Steel; Precipitation Hardening Stainless

Material Notes: Ultrachem ESR® is a chromium-nickel precipitation-hardening stainless steel, a modified PH alloy grade, which is characterized by exceptional polishability, exceptional corrosion resistance, uniform hardness in all dimensions, excellent compressive strength, simple low temperature heat treatment with small dimensional change, good weldability, excellent toughness, and excellent EDM machinability.
Ultrachem ESR® is normally supplied in a fully heat treated condition, age hardened to 38 or 42 HRC.
Ultrachem ESR®'s excellent corrosion resistance reduces both maintenance costs and production costs. Consistently high molding productivity is assured since cooling channels are not subjected to corrosion and loss of cooling efficiency.
Ultrachem ESR® is particularly suitable for applications where high surface finishes are required. It is also recommended for use in long-life molds subjected to severe working conditions, including corrosive materials and atmospheres, high stresses and indentation experienced in today's fast cycling molding operations.

Information provided by EDRO

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.280 lb/in³
@Temperature 399 °C
Prehardened to 321 HB
 0.282 lb/in³
@Temperature 199 °C
Prehardened to 321 HB
 0.284 lb/in³
@Temperature 20.0 °C
Prehardened to 321 HB
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 38 - 42
Tensile Strength, Ultimate 190000 psi
@Temperature 20.0 °C
Age hardened at 42 HRC
Tensile Strength, Yield 175000 psi
@Temperature 20.0 °C
Age hardened at 42 HRC
Elongation at Yield 14 %
@Temperature 20.0 °C
in 2"
Reduction of Area 50 %
@Temperature 20.0 °C
Modulus of Elasticity 25400 ksi
@Temperature 399 °C
 27000 ksi
@Temperature 199 °C
 28500 ksi
@Temperature 20.0 °C
Charpy Impact 25.0 ft-lb
@Temperature 20.0 °C
Age hardened at 42 HRC
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µin/in-°F
@Temperature 20.0 - 199 °C
 6.50 µin/in-°F
@Temperature 20.0 - 399 °C
Specific Heat Capacity 0.110 BTU/lb-°F
@Temperature 20.0 °C
Thermal Conductivity 112 BTU-in/hr-ft²-°F
@Temperature 20.0 °C
 129 BTU-in/hr-ft²-°F
@Temperature 199 °C
 149 BTU-in/hr-ft²-°F
@Temperature 399 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.040 %
Chromium, Cr 14.75 %
Copper, Cu 3.2 %
Iron, Fe 76.36 %As Balance
Manganese, Mn 0.50 %
Nickel, Ni 4.5 %
Niobium, Nb (Columbium, Cb) 0.25 %
Silicon, Si 0.40 %
 
Descriptive Properties
Color CodeGold

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EDRO #7 Shock Resistant S7 Tool Steel
EDRO P1FM #31 Free Machining Holder Steel
EDRO UltraChem® #15 Precipitation Hardening Stainless Mold Steel
EDRO RoyAlloy™ #6 Free Machining Stainless Holder Steel
EDRO EDRO400™ #40 Prehardened Insert Quality Martensitic Stainless Steel

NSEDRO006 / 142943

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.