MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-HS-5H-280 GSM 5 Harness Carbon Fabric
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 950-1 modified epoxy resin is a 121°C (250°F) cure system with the performance of a 177°C (350°F) curing epoxy. CYCOM 950-1 prepreg is curable under vacuum-bag-only pressure conditions. CYCOM 950-1 is a controlled flow, net resin content material that offers significant advantages over wet lay-up systems for structural repairs. Advantages include favorable stress-strain characteristics, product quality and consistency, speed of lay-up and vastly improved health and safety characteristics.

Features & Benefits:

  • Aerospace qualified
  • Low outgassing. Approved for space flight
  • Controlled flow material
  • Improved toughness compared with first- and second-generation structural epoxies
  • Dry service temperature of 150°C (300°F) when cured at 135°C (275°F)
  • Mechanical properties of a 177°C (350°F) curing material when cured at 135°C (275°F)
  • Mechanical properties to 104°C (220°F) hot/wet
  • Oven/vacuum bag cure capability as well as autoclave positive pressure cure
  • Efficient for structural repair
  • Conventional drying, lay-up, vacuum bagging and localized low-level heating is all that is required for most applications
  • Shop life of 8 weeks at ambient conditions
  • Suitable for laminate and sandwich panel usage
  • Co-curable with various aerospace qualified adhesive materials
Suggested Applications:
  • Helicopter fuselage and rotor components
  • Wing structures
  • Field repairs and permanent repairs
  • Space flight applications

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Outgassing - Total Mass Loss 0.24 %RML
 0.50 - 0.70 %TML
Collected Volatile Condensable Material 0.020 - 0.040 %
Storage Temperature <= -18.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 111000 psi
@Temperature 80.0 °C
0° orientation
 125000 psi
@Temperature 23.0 °C
90° orientation
 131000 psi
@Temperature 23.0 °C
0° orientation
Tensile Modulus 64.0 GPa
@Temperature 23.0 °C
90° orientation
 69.0 GPa
@Temperature 80.0 °C
0° orientation
 73.0 GPa
@Temperature 23.0 °C
0° orientation
Flexural Strength 124000 psi
@Temperature 80.0 °C
0° orientation
 156000 psi
@Temperature 23.0 °C
0° orientation
Flexural Modulus 62.0 GPa
@Temperature 23.0 °C
0° orientation
 64.0 GPa
@Temperature 80.0 °C
0° orientation
Compressive Strength 690 MPa
@Temperature 80.0 °C
0° orientation
 800 MPa
@Temperature 23.0 °C
90° orientation
 862 MPa
@Temperature 23.0 °C
0° orientation
Compressive Modulus 63000 MPa
@Temperature 23.0 °C
0° orientation
 64000 MPa
@Temperature 80.0 °C
0° orientation
 65000 MPa
@Temperature 23.0 °C
90° orientation
Shear Strength 8800 psi
@Temperature 80.0 °C
Interlaminar
 10600 psi
@Temperature 23.0 °C
Interlaminar
 14200 psi
@Temperature 23.0 °C
In Plane
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 220 °F
 
Processing PropertiesOriginal ValueComments
Gel Time 13.0 min
@Temperature 135 °C
Shelf Life 12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-T800-5H-280 GSM 5 Harness Carbon Fabric
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KM46J-2X2T-200
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-M46J-5H-280 GSM 5 Harness Carbon Fabric
Solvay CYCOM® 950-1 Epoxy Prepreg with 52% 120 Kevlar Fabric

PCYTED154_6 / 192667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.