MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-M46J-5H-280 GSM 5 Harness Carbon Fabric
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 950-1 modified epoxy resin is a 121°C (250°F) cure system with the performance of a 177°C (350°F) curing epoxy. CYCOM 950-1 prepreg is curable under vacuum-bag-only pressure conditions. CYCOM 950-1 is a controlled flow, net resin content material that offers significant advantages over wet lay-up systems for structural repairs. Advantages include favorable stress-strain characteristics, product quality and consistency, speed of lay-up and vastly improved health and safety characteristics.

Features & Benefits:

  • Aerospace qualified
  • Low outgassing. Approved for space flight
  • Controlled flow material
  • Improved toughness compared with first- and second-generation structural epoxies
  • Dry service temperature of 150°C (300°F) when cured at 135°C (275°F)
  • Mechanical properties of a 177°C (350°F) curing material when cured at 135°C (275°F)
  • Mechanical properties to 104°C (220°F) hot/wet
  • Oven/vacuum bag cure capability as well as autoclave positive pressure cure
  • Efficient for structural repair
  • Conventional drying, lay-up, vacuum bagging and localized low-level heating is all that is required for most applications
  • Shop life of 8 weeks at ambient conditions
  • Suitable for laminate and sandwich panel usage
  • Co-curable with various aerospace qualified adhesive materials
Suggested Applications:
  • Helicopter fuselage and rotor components
  • Wing structures
  • Field repairs and permanent repairs
  • Space flight applications

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Outgassing - Total Mass Loss 0.24 %0.24 %RML
 0.50 - 0.70 %0.50 - 0.70 %TML
Collected Volatile Condensable Material 0.020 - 0.040 %0.020 - 0.040 %
Storage Temperature <= -18.0 °C<= -0.400 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength  779 MPa
@Temperature 80.0 °C
113000 psi
@Temperature 176 °F
0° orientation
 834 MPa
@Temperature 23.0 °C
121000 psi
@Temperature 73.4 °F
0° orientation
Tensile Modulus  127 GPa
@Temperature 80.0 °C
18400 ksi
@Temperature 176 °F
0° orientation
 132 GPa
@Temperature 23.0 °C
19100 ksi
@Temperature 73.4 °F
0° orientation
Flexural Strength  593 MPa
@Temperature 123 °C
86000 psi
@Temperature 253 °F
0° orientation
 669 MPa
@Temperature 80.0 °C
97000 psi
@Temperature 176 °F
0° orientation
 731 MPa
@Temperature 23.0 °C
106000 psi
@Temperature 73.4 °F
0° orientation
Flexural Modulus  97.0 GPa
@Temperature 123 °C
14100 ksi
@Temperature 253 °F
0° orientation
 107 GPa
@Temperature 23.0 °C
15500 ksi
@Temperature 73.4 °F
0° orientation
 111 GPa
@Temperature 80.0 °C
16100 ksi
@Temperature 176 °F
0° orientation
Compressive Strength  330 MPa
@Temperature 123 °C
47900 psi
@Temperature 253 °F
0° orientation
 485 MPa
@Temperature 80.0 °C
70300 psi
@Temperature 176 °F
0° orientation
 508 MPa
@Temperature 23.0 °C
73700 psi
@Temperature 73.4 °F
0° orientation
Compressive Modulus  111 GPa
@Temperature 123 °C
16100 ksi
@Temperature 253 °F
0° orientation
 112 GPa
@Temperature 80.0 °C
16200 ksi
@Temperature 176 °F
0° orientation
 114 GPa
@Temperature 23.0 °C
16500 ksi
@Temperature 73.4 °F
0° orientation
Shear Strength  44.1 MPa
@Temperature 132 °C
6400 psi
@Temperature 270 °F
Interlaminar
 49.0 MPa
@Temperature 23.0 °C
7100 psi
@Temperature 73.4 °F
Interlaminar
 50.3 MPa
@Temperature 80.0 °C
7300 psi
@Temperature 176 °F
Interlaminar
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 104 °C220 °F
 
Processing PropertiesMetricEnglishComments
Gel Time 13.0 min
@Temperature 135 °C
13.0 min
@Temperature 275 °F
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-HS-5H-280 GSM 5 Harness Carbon Fabric
Solvay CYCOM® 950-1 Epoxy Prepreg Unidirectional Tape with 36%-M46J-140 GSM
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-M46J-Plain Weave-280 GSM
Solvay CYCOM® 950-1 Epoxy Prepreg with 42%-T800-5H-280 GSM 5 Harness Carbon Fabric

PCYTED154_9a / 192671

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.