MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene FR200000 Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Petrothene FR200000 is selected for use in the extrusion of communication grade wire and cable insulation. FR200000 is a polypropylene based, thermoplastic, low smoke, halogenated, flame retardant compound. FR200000 contributes toward meeting UL 910, CSA FT-4, UL 1666, UL 1581 and UL 444 specifications when used in conjunction with certain cable designed and jacketing materials. Applications: Wire & Cable

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.49
@Frequency 1e+6 Hz
Dissipation Factor 0.00090
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
Flammability, UL94 V-0
@Thickness 1.90 mm
Oxygen Index 26 %
 
Descriptive Properties
Processing MethodWire & Cable

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hyosung Topilene R200P PP
A. Schulman POLYFLAM™ RPP 1133 Flame Retardant, Copolymer Polypropylene
E-Polymers TEKAFIN® PH40FR Flame Retardant Heat Resistance Compounded-PP
LG Chemical LUPOL GP-3152F General Purpose Polypropylene, 15% Mineral Fillers, High Impact, Flame Retardant
Cossa Polimeri ESTAPROP 1540 GFC V0 H Flame Retardant Polypropylene, 20% Glass Filled

PEQT8817 / 220451

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.